| Raw materials | PTA + MEG |
|---|---|
| Grade | Bright/Semi-dull |
| Form | Slightly yellow/white granules |
The HCDP series contains over 10% cationic-modified monomers. In downstream applications, it is typically blended with bright polyester chips or recycled PET bottle chips in a 5:5 or 6:4 ratio, followed by drying, crystallization, melt spinning, and fiber setting to produce staple fibers or filaments.
HCDP Cationic Polyester Chips for High-Performance Blended Fibers
HCDP Cationic Polyester Chips for Staple and Filament Applications
The HCDP series contains over 10% cationic-modified monomers. In downstream applications, it is typically blended with bright polyester chips or recycled PET bottle chips in a 5:5 or 6:4 ratio, followed by drying, crystallization, melt spinning, and fiber setting to produce staple fibers or filaments.
Features
Application
Widely used in:
Specifications
| Item | Unit | HCDP | HCDP-M | HCDP-S | HCDP-EF |
| Intrinsic Viscosity | dL/g | 0.345±0.010 | 0.360±0.015 | 0.360±0.015 | 0.345±0.010 |
| Melting Point | ℃ | 205.0±5.0 | ≥185.0 | ≥185.0 | 205.0±5.0 |
| B Value | 2.0~8.0 | 2.0~8.0 | 2.0~8.0 | 2.0~8.0 | |
| L Value | ≥60.00 | ≥60.00 | ≥60.00 | ≥63.00 | |
| Carboxyl End Groups | mol/t | ≤50.0 | ≤60.0 | ≤60.0 | ≤50.0 |
| Diethylene Glycol | % | 5.5±0.5 | 6.0±0.5 | 6.0±0.5 | 5.5±0.5 |